After the pouring is completed the crucible is laid on its' side  so that any remaining metal can cool and solidify on the side  of the crucible.  If the crucible was left upright and the metal cooled in the bottom when it was next re-heated when the aluminum started to expand with the heat it might crack the crucible. 